Title Alkali-Silica Reaction of Mortar Containing Waste Glass Aggregates
Authors 박승범 ; 이봉춘 ; 권혁준
Page pp.213-220
ISSN 1229-5515
Keywords 폐유리; 알칼리 실리카 반응; 강섬유; 폴리프로필렌섬유; 퍼시멈; waste glass; alkali-silica reaction; steel fiber; polypropylene fiber; pessimum
Abstract Incorporation of wastes glass aggregate in mortar may cause crack and this may result in the strength reduction due to alkali-silica reaction(ASR) and expansion. The purposes of this study were to investigate the properties of alkali-silica expansion and strength loss through a series of experiments which had a main experimental variables such as waste glass aggregate contents, glass colors, fiber types, and fiber contents. The steel fibers and polypropylene fibers were used for constraining the ASR expansion and mortar cracking. From the result, green waste glass was more suitable than brown one because of low expansion. And in this accelerated ASTM C 1260 test of waste glass, pessimum content can not be found. Also, when used the fibers with waste glass, there is an effect on reduction of expansion and strength loss due to ASR between the alkali in the cement paste and the silica in the waste glass. Specially, adding 1.5 vol.% of steel fiber to 20% of waste glass, the expansion ratio was reduced by 40% and flexural strength was developed by up to 110% comparing with only waste glass(80℃ H₂O curing).